Conditioning
Laminate, substrate, backing laminate and glue
should be conditioned for at least 48 hours prior fabrication,
having all the components at room temperature not below
18°C, in a dry storage area with humidity between 45
and 55% .
During these 48 hours the various components will have the
time to reach equal or very close humidity contents. Starting
from very similar conditions will limit the differences
in dimensional stability and by consequence the risk of
warping of the fabricated element.
Wooden subtrates should have a humidity close to 10%. Decorative laminate and backing laminate should have the same moisture content. |
|
|